Monomer |
Structure |
MW (g/mol) |
Tg (°C) |
Methyl Acrylate (MA) |
|
86.1 |
7 |
Acrylic acid (AA) |
|
72.1 |
101 |
n-Butyl acrylate (n-BA) |
|
128.2 |
-53 |
Lauryl acrylate (LA) |
|
247 |
-5 |
Stearyl acrylate (SA) |
|
324 |
38 |
Benzyl acrylate (BNA) |
|
162 |
6 |
Cyclohexyl acrylate (CHA) |
|
154.2 |
16 |
Isobornyl acrylate (IBOA) |
|
208.3 |
94 |
2-Ethylhexyl acrylate (2-EHA) |
|
184.3 |
-50 |
Tetrahydrofurfuryl acrylate (THFA) |
|
156.2 |
-14 |
2-Hydroxyethyl acrylate (HEA) |
|
116.1 |
-14 |